AASHTO M 203M/M 203-12 (2016) covers two types and two grades of seven-wire, uncoated steel strand for use in pretensioned and post-tensioned prestressed concrete construction. The two types of strand are low-relaxation and stress-relieved (normal-relaxation). Low-relaxation strand shall be regarded as the standard type. Stress-relieved (normal-relaxation) strand will not be furnished unless specifically ordered, or by arrangement between purchaser and supplier. Grade 1725 [250] and Grade 1860 [270] have minimum ultimate strengths of 1725 MPa [250 ksi] and 1860 MPa [270 ksi], respectively, based on the nominal area of the strand.
 

Document History

  1. AASHTO M 203M/M 203-20


    Standard Specification for Steel Strand, Uncoated Seven-Wire for Concrete Reinforcement (ASTM A 416/A 416M-18)

    • Most Recent
  2. AASHTO M 203M/M 203-18


    Standard Specification for Steel Strand, Uncoated Seven-Wire for Concrete Reinforcement (ASTM A 416/A 416M-17)

    • Historical Version
  3. AASHTO M 203M/M 203-12 (2016)

    👀currently
    viewing


    Standard Specification for Steel Strand, Uncoated Seven-Wire for Concrete Reinforcement (ASTM A 416/A 416M-10)

    • Historical Version
  4. AASHTO M 203M/M 203-05


    Standard Specification for Steel Strand, Uncoated Seven-Wire for Concrete Reinforcement

    • Historical Version